Alloy Digest (1953) 2 (4): Cu-7.
Published: 01 April 1953
... HY-TEN-SL No. 1 is a close-grained, tough, homogeneous metal, having the non-corrosive properties of bronze and the strength of alloy steel. It has good wear resisting qualities under heavy or shock loads. This datasheet provides information on composition, physical properties, hardness...