Alloy Digest (1960) 9 (9): SA-103.
Published: 01 September 1960
... HY-TEN B TEMPER No. 3-X is a strong, tough alloy steel of high hardenability recommended for heavy duty applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on...
Journal Articles
Alloy Digest (1970) 19 (1): SA-248.
Published: 01 January 1970
... HY-TEN B Temper No. 3X-40 is a medium-carbon alloy steel having free-cutting characteristics. It is recommended for machine tools, mining and road building equipment, gears, crankshafts, bolts, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and...