Alloy Digest (1963) 12 (8): TS-136.
Published: 01 August 1963
... HWD-2 is a chromium-molybdenum-vanadium hot work steel particularly useful for hot work die operations that are water-cooled in service. It is particularly useful for die casting, extrusion and forging dies. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1962) 11 (4): TS-117.
Published: 01 April 1962
... HWD No. 1 is a chromium-molybdenum-tungsten alloy hot work steel developed for applications where dies or tools are subject to heavy pressure or impact while in contact with hot metal. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1958) 7 (7): TS-72.
Published: 01 July 1958
... HWD No. 3 is an air-hardening hot work steel recommended for dies where a minimum amount of distortion during hardening is required. It is equivalent to AISI Type H13. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and creep...
Journal Articles
Alloy Digest (1961) 10 (11): TS-111.
Published: 01 November 1961
... Potomac M Pressurdie No 3 No. 883 Vanadium Firedie HWD No. 3 Dica B. Vanadium VDC Tbermold AV Vulcast Hotform 3 General Characteristics: Cutting Speeds, sfpm High Speed Cemented mSteA Carbide 58-66 240-280 48-54 200-230 40-46 180-195 34-38 150-170 Crucible Allegheny Ludlum Braebum Carpenter Columbia Fir...
Journal Articles
Alloy Digest (1959) 8 (11): TS-86.
Published: 01 November 1959
... Equivalents: AISI Type H13 SAE Type H13 Pressurdie 3 Braeburn Nu-Die V Crucible Poromac M V. D. C. HWD No. 3 CromoHigh V Dica B. Vanadium Thermold AV VLdarSr Vanadium Die Cast All;o&;ny-Ludlum Fitth Sterling Bethlehem Jessop Universal Cyclops Vulcan-Ridd Columbia General Characteristics: Carpenter No. 883...
Journal Articles
Alloy Digest (1962) 11 (1): TS-113.
Published: 01 January 1962
... 240-280 l/l6 l/32 48-54 200.230 l/8 l/32 40-46 MO-195 l/4 l/32 34-38 120-170 l Woldman 81 Gibbons: Machinability & Machiaiog of Metals. Specification Equivalent: AISI Type HI3 SAE Type H13 Pressuredie 3 Nu-Die V Potomac M V.D.C. HWD No. 3 Cromo-High V Dica B. Vaaadium Thermold AV Vulcast Vanadium Die...