Alloy Digest (1984) 33 (10): TS-429.
Published: 01 October 1984
... HS-100 is a super high-speed steel built on an AISI Type M33 base but with higher carbon and cobalt. It is able to attain an approximate hardness of Rockwell C 68 with normal heat treatment. It gains its great resistance to wear from its high hardness rather than from excess vanadium carbides. HS...
Journal Articles
Alloy Digest (1964) 13 (5): CI-33.
Published: 01 May 1964
... in the form of nodules or spheroids. Ir possesses unusually high ducciliry, strength and casrabilicy. It is furnished in three different grades, namely, SF-60, SP-SO and SH-100. Alloyed grades are also available under different designations as AQS-HS and WS. *Registered Trade Mark. Composition: Physical...
Journal Articles
Alloy Digest (1998) 47 (8): Fe-118.
Published: 01 August 1998
...-1420 F) for 2 h in dry hydrogen at- mosphere or a high vacuum. Cool at 100-500 C (I 8&900 F) per hour to room temperature. Workability: Hot Working. Hiperco Alloy 27 HS can be forged from 1175-1205 C (2150-2200 OF). The heating time should be about one hour for each inch of thickness. Following...
Journal Articles
Alloy Digest (2010) 59 (8): SS-1074.
Published: 01 August 2010
... Sandvik T302 HS is a general purpose austenitic stainless steel with respect to corrosion resistance only in a spring temper for higher strength. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear and bend strength It also includes...
Journal Articles
Alloy Digest (2002) 51 (11): SS-868.
Published: 01 November 2002
... Staballoy AG 17 HS is an improved version of Staballoy AG 17 (see Alloy Digest SS-857, July 2002) with similar characteristics, but with higher yield strength and better fatigue properties. Applications include critical nonmagnetic drill stem components. This datasheet provides information...
Journal Articles
Alloy Digest (1977) 26 (11): SA-338.
Published: 01 November 1977
... 0.0037 117 AISI 41 LAO Annealed 67 128 0.0043 159 Competitive Grade 49 109 0.0037 117 DYNA-LOY HS-32 60 121 0.0041 142 *Based on 100 for free-machining AK1 1211 steel. **Based on I -inch wide form tool. TFeed rate for !4 + !; drill - rough form tool rate is ?,i to ?; that of drill. f?Production rate...
Journal Articles
Alloy Digest (1969) 18 (12): TS-225.
Published: 01 December 1969
... tungstenchromium-vanadium content, Special HS-55 can be machined without undue difficulty. However, it does not machine as readily as the lower-alloyed grades. Special HS-55 is rated at 65. as compared with a 1 percent carbon tool steel rated at 100. In machining this steel with high-speed steel cutters, grind...
Journal Articles
Alloy Digest (1999) 48 (7): Ni-556.
Published: 01 July 1999
... Carpenter 20Mo-6 HS is an alloy in the generic family of 6% molybdenum alloys, which are very corrosion resistant. This steel also possesses an excellent resistance to environmental cracking. (See also Carpenter 20Mo-6, Alloy Digest SS-444, May 1984.) This datasheet provides information...
Journal Articles
Alloy Digest (2006) 55 (12): TS-639.
Published: 01 December 2006
...) Coefficient of linear thermal expansion, 10 6/K (10 6/°F) 40 260 °C (100 500 °F) 11.5 (6.40) 40 425 °C (100 800 °F) 11.8 (6.58) 40 540 °C (100 1000 °F) 12.1 (6.72) CPM® REX® M4 HC (HS) Filing Code: TS-639 Tool Steel December 2006 CPM® REX® M4 HC (HS) (High-Speed Steel) Crucible CPM Rex M4 HC (HS) is a high...
Journal Articles
Alloy Digest (1996) 45 (12): TS-548.
Published: 01 December 1996
...). It is customary to use two furnaces to harden Carpenter Micro-Melt HS-30 alloy. One furnace is used to preheat the workpiece to 1500/1550°F (816/843 C), and the second is used to rapidly heat the workpiece 6om the preheating temperature to the hardening temperature of 2125/22OO F 212 100 6.6 1188 500 260 6.8...
Journal Articles
Alloy Digest (2003) 52 (1): SS-870.
Published: 01 January 2003
... Staballoy 734 HS is an austenitic stainless steel with enhanced strength and corrosion resistance and is a stronger version of Staballoy 734 (see Alloy Digest SS-860, August 2002). This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1961) 10 (7): SA-117.
Published: 01 July 1961
... HS-260 is a high strength steel designed for minimum tensile strength level of 260,000 psi in the heat treated condition. It exhibits good ductility and impact values consistent with the high hardness. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1953) 2 (1): SA-5.
Published: 01 January 1953
.... 60000 max. 70000 min. 45000 min. 45000 max. 50000 min. 27 30 22 mio. 120 - 105 45000 48000 75-88 6075 85-90 Tablo 2 LOW TEMPERATURE CHARPY IMPACT (Yoloy Gr. Temperahue F HS) (Normalized before machining) Charpy Impact, ft. Ibs. V-Notch 70 130 32 130 0 ,128 -25 125 -50 115 -75 95 -100 70 Heat Treatmenti...
Journal Articles
Alloy Digest (2003) 52 (5): SS-884.
Published: 01 May 2003
.../asm.ad.ss0884 Table 2 Typical Machining Speeds and Feeds Tool material Speed, fpm Feed, ipr Tool material Speed, fpm Feed, ipr Turning, single-point and box tools Micro-Melt Powder HS, M48, T15 Depth of cut, in., 0.150 171 0.0180 Depth of cut, in., 0.025 202 0.0084 Carbide C2, uncoated, depth of cut, in., 0.150...
Journal Articles
Alloy Digest (2003) 52 (4): SS-882.
Published: 01 April 2003
... 75 55 68 50 704 1300 517 75 655 95 21 60 187 92 HRB 108 80 102 75 25.4 mm (1 in.) round bar, hardened at 982 °C (1800 °F) 1/2 hour, oil quenched and tempered 2 h Rough reaming (continued) Micro-Melt Powder HS, M48, T15 (continued) Table 2 Typical Machining Speeds and Feeds Tool material Speed, fpm...
Journal Articles
Alloy Digest (2011) 60 (8): SS-1100.
Published: 01 August 2011
... are susceptible to stress corrosion cracking (SCC) when in contact with chloride solutions at elevated temperatures. Specification Equivalents: Sandvik Grade Bioline Sandvik 11R51 HV ASTM 302 Mod. ISO X9 CrNi 17-8 Grade 1 HS EN 1.4310 HS EN Name X9 CrNi 17-8 HS JIS SUS 302 Mod. The grade designations, except...
Journal Articles
Alloy Digest (2003) 52 (2): SS-875.
Published: 01 February 2003
... Feed, ipr Tool material Speed, fpm Feed, ipr Turning, single-point and box tools Micro-Melt Powder HS, M48, T15 Depth of cut 0.150 in. 140 0.0180 Depth of cut 0.025 in. 171 0.0084 Carbide C2, uncoated, depth of cut 0.150 in. 470 0.0180 Carbide C2, coated, depth of cut 0.150 in. 600 0.0180 Carbide C3...
Journal Articles
Alloy Digest (2011) 60 (9): SS-1102.
Published: 01 September 2011
... 420 ISO X9 CrNi 17-8 Grade 1 HS EN 1.2028/1.4310 EN Name X35 Cr 14 JIS SUS 302 Mod. W.Nr. 1.4007 SS 2304 AFNOR Z30C13 (13H) The grade designations, except for EN 1.4310 HS, referred to above are nearest equivalents. Product standard EN 10270-3 ASTM A313/A313M General Characteristics: Sandvik Bioline...
Journal Articles
Alloy Digest (2003) 52 (3): SS-878.
Published: 01 March 2003
...: Carpenter Specialty Alloys Reading, PA 19612 (610) 208-2000 (800) 654-6543 ISSN: 002-614X SS-878B Table 3 Typical Machining Speeds and Feeds Tool material Speed, fpm Feed, ipr Tool material Speed, fpm Feed, ipr Turning, single-point and box tools Micro-Melt Powder HS, M48, T15 Depth of cut, in., 0.150 140...
Journal Articles
Alloy Digest (2003) 52 (6): SS-886.
Published: 01 June 2003
... Speeds and Feeds for Turning with Single-Point and Box Tools Tool material Depth of cut, in. Speed, fpm Feed, ipr Tool material Depth of cut, in. Speed, fpm Feed, ipr Solution-treated or double-aged H1150-M Micro-Melt Powder HS M48, T15 0.150 90 0.015 0.025 105 0.007 Carbide C6, uncoated 0.150 375 0.015...