Alloy Digest (2004) 53 (11): CS-144.
Published: 01 November 2004
.... Copyright © ASM International® 2004 2004 ASM International chemical composition heat treatability HP Magnet Plate Steel joinability machinability magnetic permeability physical properties tensile properties workability UNS G10060 Chemical Composition, wt Carbon 0.08 max Manganese 0.25...
Journal Articles
Alloy Digest (2019) 68 (6): SA-847.
Published: 01 June 2019
...: ArcelorMittal USA. Producer or Source: ArcelorMittal USA Copyright © ASM International® 2019 2019 ASM International chemical composition heat treatability HP magnet steel joinability machinability magnet steel shear strength tensile properties Arcelor Mittal HP magnet plate was developed...
Journal Articles
Alloy Digest (2021) 70 (3): SS-1332.
Published: 01 March 2021
... performs ATI 201 HP is not recommended for service conditions where temperatures above 815 °C (1500 °F) are encountered. adequately as a replacement for type 301 austenitic stainless steel in most mild environments. Hot Forming Non-magnetic in the annealed condition but becomes magnetic when cold worked...
Journal Articles
Alloy Digest (2013) 62 (7): SS-1150.
Published: 01 July 2013
... Columbium 0.3 + (9 × C) min Titanium 0.10 min 0.50 max Nitrogen 0.030 Iron bal Physical Properties: ATI 441 alloy is a single-phase ferritic (body centered cubic) stainless steel at all temperatures up to the melting point. Density, kg/m3 (lb/in.) 7711 (0.278) Magnetic permeability Ferromagnetic Mean...
Journal Articles
Alloy Digest (1959) 8 (7): Ti-20.
Published: 01 July 1959
... grade of commercially pure titanium for applications requiring maximum ductility and formabiiiy. Its strength is about the same as that of fully annealed austenitic stainiess steeL It has good impact strength at low temperatures as Rem-Cru A-40.) (Previously known Forms Available: Sheet, strip, plate...
Journal Articles
Alloy Digest (2002) 51 (11): Ni-594.
Published: 01 November 2002
... Tantalum 3.15 4.15 Titanium 0.40 max Aluminum 0.40 max Cobalt 1.0 max Iron 5.0 max Nitrogen 0.02 max Nickel bal (58.0 min) Physical Properties: Density, kg/m3 (lb/in.3 ) 8440 (0.305) Specific heat capacity, 410 (0.098) J/kg K (Btu/lb °F) Melting range, °C (°F) 1280 1350 (2350 2460) Magnetic...
Journal Articles
Alloy Digest (1977) 26 (11): SS-228.
Published: 01 November 1977
... kilns chemical composition corrosion-resistant alloys creep properties elasticity fatigue properties furnace tubes heat treatability heat-treating furnaces joinability machinability physical properties SUPERTHERM tensile properties Filing Code: SS-228 Stainless Steel SUPERTHERM Revised...