1-9 of 9 Search Results for

HIPERCO

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1964) 13 (7): Fe-26.
Published: 01 July 1964
... Hiperco 27 is an iron-cobalt type of soft magnetic material recommended for use in motors, generators, transformers and relays and at temperatures above 950 F. It is used for high flux levels. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1967) 16 (1): Co-50.
Published: 01 January 1967
... Hiperco 50 is a cobalt-iron-vanadium soft magnetic alloy for high flux levels. It has high permeability at high inductions and low d-c coercive force. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2002) 51 (10): Fe-124.
Published: 01 October 2002
... Hiperco Alloy 15 is a development in soft magnetic alloys that combines the properties of high saturation, magnetization, high electrical resistivity, and lower cobalt content. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1998) 47 (6): Co-105.
Published: 01 June 1998
... Hiperco 50HS is an improved soft magnetic alloy with a finer grain size that produces greater strengths than those found in Hiperco 50 (Alloy Digest Co-83, February 1988). This datasheet provides information on composition, physical properties, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1998) 47 (8): Fe-118.
Published: 01 August 1998
... Hiperco Alloy 27 HS is a soft magnetic material that combines high magnetic saturation with high yield stress. The alloy is a candidate for use in magnetic-thrust bearings, fly wheels, and shafts requiring the above combination. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1999) 48 (11): Co-107.
Published: 01 November 1999
... Hiperco 50A is an iron-cobalt-vanadium soft magnetic alloy possessing high magnetic saturation, high direct current (dc) maximum permeability, low dc coercive force, and low alternating current (ac) core loss. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1988) 37 (2): Co-83.
Published: 01 February 1988
... CARPENTER HIPERCO 50 is a magnetic soft alloy used primarily as magnetic core in electrical equipment requiring high permeability at very high magnetic flux densities. These magnetic characteristics permit weight reduction, reduction of copper turns and insulation in the end product in comparison...
Journal Articles
Alloy Digest (1970) 19 (1): Fe-41.
Published: 01 January 1970
... Hiperco 35 is an iron-cobalt type of soft magnetic material recommended for use in motors, generators, transformers and relays at temperature above 950 F. It yields the highest known saturation value of 24,500 gausses. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1957) 6 (4): Fe-13.
Published: 01 April 1957
... HIPERCO is a magnetic alloy having a high magnetic saturation value. It permits the design of motors with less metal for the same power, or more power from the same amount of metal. This datasheet provides information on composition, physical properties, and tensile properties. It also includes...