Journal Articles
Alloy Digest (1995) 44 (6): Cu-601.
Published: 01 June 1995
... HIDURON alloy 191 was developed for marine applications where both a combination of strength and good corrosion/ impingement resistance is needed. It finds applications in shafts, fasteners and valve stems. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2006) 55 (6): Cu-744.
Published: 01 June 2006
...-Al bronze 247 36 0.075 4.3 Hiduron 191 425 62 0.02 4.8 DOI: 10.31399/asm.ad.cu0744 Applications: Defense applications include control elements of submarines, pump shafts, mechanical seals, gears, hose couplings, propeller shafts, and drive bushes. The alloy is used as tubes and tube plates for heavy...
Journal Articles
Alloy Digest (2006) 55 (5): Cu-743.
Published: 01 May 2006
... for 2 h; results obtained from 25 mm rolled bar Table 2 Typical Mechanical Properties Alloy Comparison Yield strength, 0.2% Tensile strength MPa ksi MPa ksi Elongation on 5.65 _ So, % Hiduron 130, to DTD 900/4805 680 99 880 128 12 Hiduron 191 510 74 800 116 25 Nickel aluminum bronze to DGS 1043 310 45...
Journal Articles
Alloy Digest (1995) 44 (7): Cu-602.
Published: 01 July 1995
.... General Characteristics: With mechanical strength matching that of B7 steel and a re- sistance to corrosion similar to that of established high strength cupronickel, HIDURON alloy 191 (Alloy Digest Cu-601) from which it has been developed, MARINEL alloy is ideal for bolting and other critical high...