Publisher: Journals Gateway
Alloy Digest (2006) 55 (10): Cu-747.
Published: 01 October 2006
... Hidurel 640 is a copper alloy with similar properties to Hidurel 6 (see Alloy Digest Cu-746, September 2006) with superior mechanical properties at high temperature. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear...