Journal Articles
Alloy Digest (1996) 45 (7): Cu-607.
Published: 01 July 1996
... Hidurel 5 is a precipitation-hardening copper-nickel-silicon bronze alloy with high conductivity and strength, corrosion resistance to marine environments and hydrogen embrittlement, and good antifrictional properties. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2006) 55 (9): Cu-746.
Published: 01 September 2006
... Hidurel 6 is a copper alloy with some chromium. It has high strength with high conductivity. The alloy has superior conductivity to Hidurel 5 (Alloy Digest Cu-607, July 1996) and is used for electrical applications where strength and brazing ability are major requirements. This datasheet provides...
Journal Articles
Alloy Digest (2006) 55 (10): Cu-747.
Published: 01 October 2006
... Thermal conductivity MPa ksi J ft . lbf Electrical conductivity, %IACS W/m . K Btu/(ft . h . ┬░F) Nickel-aluminum bronze 247 36 23 17 8 41 24 Aluminum-silicon bronze 220 32 33 24 9 41 24 70/30 copper-nickel 115 17 54 40 5 30 17 Hidurel 6 216 31 34 25 80 330 191 DOI: 10.31399/asm.ad.cu0747 Specifications...