1-1 of 1 Search Results for

HI-QUA-LED 43L40

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1966) 15 (2): SA-191.
Published: 01 February 1966
... HI-QUA-LED 43L40 is a free-machining nickel, chromium, molybdenum alloy steel having high hardenability. It is oil hardening and exhibits combination of high tensile and endurance strengths along with ductility and toughness. This datasheet provides information on composition, physical properties...