Journal Articles
Alloy Digest (1966) 15 (11): SA-204.
Published: 01 November 1966
... HECLA EM, 20 is an iron-nickel-cobalt-chromium austenitic alloy steel having high oxidation and scaling resistance. It is recommended for high temperature service and medium loads up to 2000 F, such as turbine blading, jet engine exhaust stacks and combustion chambers. This datasheet provides...