Alloy Digest (1974) 23 (11): Ni-211.
Published: 01 November 1974
... HASTELLOY Alloy C-4 is a nickel-chromium-molybdenum alloy with outstanding high-temperature stability as shown by high ductility and corrosion resistance even after long-time aging in the range 1200-1900 F. Alloy C-4 also has excellent resistance to stress-corrosion cracking and to oxidizing...
Journal Articles
Alloy Digest (1989) 38 (1): Ni-367.
Published: 01 January 1989
... UNS N06455 workability UNS N06455 Filing Code: Nickel Alloy Ni-367 -DIGEST JANUARY 1999 - DATA ON WORLD WIDE METALS AND ALLOYS ~l~&Y~heAlriOhb-. P-by: Aby Diga. lnc./zol-e77-9181 z~ebbussdk 27CSmfmldSimat.ORllge,NJ.07050/U.S.A UNS NO6455 (Nickel-Chromium Alloy: Hastelloy 64) UNS NO6455...
Journal Articles
Alloy Digest (2004) 53 (6): Ni-621.
Published: 01 June 2004
... Hastelloy C-22HS has, like the other C-type alloys, excellent corrosion resistance, but it also exhibits high strength, nearly double the other alloys in the family. (See updated datasheet Alloy Digest Ni-742, March 2018.) This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1996) 45 (9): Ni-516.
Published: 01 September 1996
... Hastelloy C-2000 has a broad capability range for handling corrosive environments. The alloy has high resistance to reagent grade sulfuric acid, hydrochloric acid to high concentrations, and nitric acid. The alloy has outstanding localized corrosion resistance, excellent stress-corrosion cracking...
Journal Articles
Alloy Digest (1993) 42 (8): Ni-440.
Published: 01 August 1993
... HASTELLOY alloy C-276 is a solid solution, nickel-molybdenum-chromium alloy, with outstanding resistance to localized corrosion and to both oxidizing and reducing media. (See Alloy Digest Ni-164, May 1971, for base metal.) This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1985) 34 (7): Ni-317.
Published: 01 July 1985
... HASTELLOY Alloy C-22 is a nickel-chromium-molybdenum alloy that has outstanding resistance to pitting, crevice corrosion and stress-corrosion cracking. The alloy also has excellent resistance to both reducing and oxidizing media. The alloy has good mechanical properties at both room and elevated...
Journal Articles
Alloy Digest (2018) 67 (3): Ni-742.
Published: 01 March 2018
... Hastelloy C-22HS is a Ni-Cr-Mo alloy that exhibits an exceptional combination of mechanical properties and corrosion resistance in the cold-worked (CW) condition. This is an updated revision of Alloy Digest Ni-621, June 2004. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1985) 34 (9): Ni-322.
Published: 01 September 1985
... Reduction (2 in.) of Area 9% 9% 60 70 56 60 36 43 37 40 Table 4 - COMMERCIAL PHOSPHORIC ACID CORROSION DATA [Acids from several manufacturers at 241 OF (I 16 C)] Acid Test Environment 44% P205 44% P20~ + 2000 ppm Cl 44% P205 + 0.5% HF 52% P20~ 54% P?OS Average Corrosion Rate, Mils/yr (mm/yr) Alloy G-30...
Journal Articles
Alloy Digest (1993) 42 (2): Ni-423.
Published: 01 February 1993
... ILS. and 700 mi CO. (pressure at temu Extension Rate: 4 x 10-6/set. 300 350 425 450 . 1 L. . 1 _ Time E / lime A Elongation; /Elongation A ROA EIROAA 1.06 1.06 0.98 1.25 1.16 0.90 1.06 1.05 1.00 1.44 1.00 0.87 Table 9 - C-RING DATA COLD WORKED G-5p ALLOY C-RING RESULTS Actual Stress 100% -No Cracking...
Journal Articles
Alloy Digest (1994) 43 (9): Ni-464.
Published: 01 September 1994
...; NM64 - DIGEST- SEPTEMBER 1994 DATA ON WORLD WIDE METALS AND ALLOYS ocqyrigJy199d.mlyDk.AlllighLsnrserved p-by: AlbyDi Inc/201477-9161 Lmshmmprerypicpr.noftob8uredfor 27CanlieldStmel.Orarq.N.J.07050/U.SA speaiiicaba, Q hal c&s@. HASTELLOY@ D-20P ALLOY (Corrosion-resistant nickel-base alloy) HASTELLOY@ D...
Journal Articles
Alloy Digest (1999) 48 (5): Ni-552.
Published: 01 May 1999
...- mended. 4. Covered electrodes used from an unopened can require no fur- ther drying. Unused electrodes should be stored and dispensed from a temperature-controlled oven held in the range 121 200 °C (250 400 °F). Avoid room temperature exposure, as mois- ture pickup will lower mechanical properties. 5...
Journal Articles
Alloy Digest (2004) 53 (7): Ni-622.
Published: 01 July 2004
... consists of heating at 1177 °C (2150 °F) and rapidly air cooling or water quenching. Hot-formed parts should be given this treatment prior to final fabrication or installation. Workability: This alloy can be fabricated using the same techniques as for Hastelloys G-3 and G-30. For detailed information...
Journal Articles
Alloy Digest (1956) 5 (2): Ni-23.
Published: 01 February 1956
... HASTELLOY alloy-C is a nickel-molybdenum-chromium-iron alloy, highly resistant to strongly oxidizing acids, acid mixtures, and salts as well as chlorine and chlorine-bearing compounds, and with excellent properties as high temperatures. The strength and oxidation resistance at elevated...
Journal Articles
Alloy Digest (1971) 20 (5): Ni-164.
Published: 01 May 1971
... HASTELLOY Alloy C-276 is an improved version of Hastelloy Alloy C with the same excellent corrosion resistance and greatly improved fabric-ability. It also has excellent high temperature properties. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (1994) 43 (8): Ni-461.
Published: 01 August 1994
... >20,000 1587 0.333 (9.22) *To convert mils per year (mpy) to mm per year, divide by 40. DOI: 10.31399/asm.ad.ni0461 Copyright © ASM International® 1996 COMPARISON OF T-T-T CHARACTERISTICS 700°C TENSILE ELONGATION 530 0.01 0.1 1 10 loo Fig. 1 - Thermal stability 60, Fig. 2 - Tensile elongation at 700...
Journal Articles
Alloy Digest (2015) 64 (12): SS-1234.
Published: 01 December 2015
... or Hastelloy C. Product Forms Available: Plate, sheet, and strip. See size availability in Fig. 4. Applications: Seawater heat exchanger, desalinization of seawater plant, salt manufacture equipment, paper manufacturing plant, pulp bleaching equipment, exhaust gas desulfurizer, acid- proof apparatus, various...
Journal Articles
Alloy Digest (2010) 59 (5): Ni-679.
Published: 01 May 2010
... rolled shells. No anneal is necessary for cold rolled vessel shells. Corrosion Resistance: This is a nickel alloy with superior resistance to hydrochloric and sulfuric acid while also having excellent sea and crevice corrosion. See Tables 3 and 4. Hastelloy, Hybrid-BC1, C-2000, and B3 are registered...
Journal Articles
Alloy Digest (1993) 42 (4): Ni-425.
Published: 01 April 1993
... cov- l ZLmpaatme range of 100@15oo F (S38-816OC) shonld be avoided. Postwdd stxess relieving in the UXPF (6Sm range will case embritdemmt and poMible necldag of the alloy. The only heat ueaenmt which is xccomnmdedforalloyB2isa fun solutial anneal at 195oT (1065 C) for an appr@aR tim followed...
Journal Articles
Alloy Digest (1960) 9 (2): Ni-55.
Published: 01 February 1960
... r&stance and freedom from aging embrittlement. ComEEn: 0.04 - 0.08 Physical Constants: Specific gravity 8.79 c%mmium 6.00 - 8.00 Density, lb/cu.in. 0.317 Molybdenum 15.OO-18.00 Melting range, F 2370-2430 Iron 5.00 max. Electrical resistivity, microhm-cm 139 Manganese 0.8 max. Aluminum + Ti Thermal...
Journal Articles
Alloy Digest (1956) 5 (12): Ni-30.
Published: 01 December 1956
...% at temperatures to 176 deg. F. The high chromium content increases its passivity when air or oxidizers are present in the acid. Boiling phosphoric acid at concentrations up to 70% can be handled successfully. Corrosion rates will, of course, be a&c-ted when dissolved copper or other metallic ions that inhibit...