Alloy Digest (1988) 37 (12): Ni-365.
Published: 01 December 1988
... International® 1996 1996 ASM International chemical composition corrosion-resistant alloys corrosivity elasticity HASTELLOY ALLOY H-9 M heat treatability joinability machinability physical properties tensile properties workability DECEMBER 1999 -DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS...
Journal Articles
Alloy Digest (1994) 43 (8): Ni-461.
Published: 01 August 1994
... max. 3.0 max. 0.10 max. Physical Constants: Density, lb/m. @n/cc) PROPERTIES Table 1 - TYPICAL ROOM TEMPERATURE TENSILE PROPERTIES Thickness Ultimate Tensile (in) Strength (Ksi) 0.125 129.0 0.250 128.7 0.500 131.5 1.00 130.5 Yield Strength Elongation 0.2% Offset (Ksi) in 2 in. (9%) 64.5 57.5 63.0 58.2...
Journal Articles
Alloy Digest (1996) 45 (9): Ni-516.
Published: 01 September 1996
.... 0.08 max. Balance Physical Properties: Density at room temperatnre. lb/ii3 (s/cm3) 0.307 (8.50) Thermal conductivity. Btu . in II. OF (W/m. K) At room temperature 63 (9.1) At 2OO F (lOO=C) 74 (10.8) At 600°F (3OO C) 99 (14.1) At 1000°F (500°C) 133 (18.0) At 14OO F (700°C) 180 (24.8) At 18OO F (9oooC...
Journal Articles
Alloy Digest (1994) 43 (9): Ni-464.
Published: 01 September 1994
...% H$O, + 42 g/l Fez (SO Table 2 -CRITICAL PITTING TEMPERATURE 4% NaCl + 0.1% F%(SO& + 0.01 M HCI MOY D-205 2OCB-3@ 316LSS Fe-17Cr- 2ONi-5Si Temperature C F 30 86 25 68 25 68 10 50 Table 3 - STRESS CORROSION CRACKING 45% MgC&, 154°C (309 F) Time to Failure Alloy Hours D-205 >1008* C-276 >1008* 254...
Journal Articles
Alloy Digest (1956) 5 (2): Ni-23.
Published: 01 February 1956
...-magnetic) M appmx. 1.000 to 1.001 l Re&ered trade-mark of Union Carbide and Carbon Gxporacion. PROPERTIES Table 1 - TYPICAL CAST PROPERTIES (ANNEALED) Tensile suength, psi 72000-80000 Yield saength, psi ( 0.2% ) Elongation, % in 2" 450Eooo Reduaion of m % 11-16 BrineII hardness 175.215 Id impace, ft lbs...
Journal Articles
Alloy Digest (1971) 20 (5): Ni-164.
Published: 01 May 1971
... properties workability Filing Code: Ni-194 HASTELLOY Alloy C-276 Nicke A w MAY 1971 DIGESTa - DATA ON WORLD WIDE METALS AND ALLOYS Pvbiisbsd by Engineering Alloys Digest. Inc. Upper Mondair. New Jersey H ASTEL LOY * Alloy C-276 (Corrosion and Heat Resisting Alloy) HASTELLOY Alloy C-276 is an improved...
Journal Articles
Alloy Digest (1993) 42 (2): Ni-423.
Published: 01 February 1993
... Sigma 0.11 0.08 No. of Testr 26 24 ElongationE/ElongationA aIloy G-3 G-50 alloy (3ooOF) (35OO F) 0.92 1.11 0.66 0.93 1.16 1.37 0.12 0.10 26 24 ROAEIROAA alloy G-3 G-50 alloy (3@m (350°F) 1.04 0.98 0.65 0.88 1.18 1.02 0.10 0.03 26 24 Table 8 -TYPICAL SSRT DATA FOR G-50 ALLOY Envimnment - 20% NaCl. 75 mi...
Journal Articles
Alloy Digest (1971) 20 (4): Co-63.
Published: 01 April 1971
... Layer that forms on the surface is adherent and has a high melting point. MAR-M 9 18 has approximately the same resistance to static air oxidation as nickel-base Hastelloy alloy X and is markedly superior to cobalt-base alloy L 605. Comparative rates of oxidation at 21000F for the three materials...
Journal Articles
Alloy Digest (1956) 5 (12): Ni-30.
Published: 01 December 1956
... Carbide and Carbon &pration. Composition: Nominal Physical Constants: carbon IrOll ;:I specsc gravity Density, lb./cu. in. &5 ChromiUlll 2 Thermal coef. expansion per OF. 68-2000~. 0.0000081 Molybdenum 68-1000°F. 0.0000089 fZo;oAm + Ta 2 o.ooooo95 0.5 min. p;m;; Manganese 1.5 Electrical rektanrr &rohm...
Journal Articles
Alloy Digest (1985) 34 (8): Ni-320.
Published: 01 August 1985
... properties elasticity HAYNES ALLOY No. 230 heat treatability high-temperature alloys joinability oxidation resistance physical properties tensile properties thermal stability workability AUGUST 1995 - DATA ON WORLD WIDE METALS AND ALLOYS - Published hv m Copyright 1985. Alloy Digest. Inc. All...
Journal Articles
Alloy Digest (1954) 3 (12): Ni-14.
Published: 01 December 1954
... chemical composition creep properties Hastelloy alloy X heat treatability machinability physical properties tensile properties workability Filing Code: Ni-14 HASTELLOY ALLOY X Nidcd Alloy DECEMBER 1954 m DATA ON WORLD WIDE METALS AND ALLOYS Pvbhbd by rhgharing Auoy Digas& Inc. Uppa Mona& New Jw...
Journal Articles
Alloy Digest (1998) 47 (2): Co-104.
Published: 01 February 1998
... -Dy:A.sM- A&terlab Park, ohi0 440734XlO2 uo-336-5151 Fax- h&m-.Smv@po~lnU.cug ANVAL@ ULTIMEl @ (Cobalt-Base Weld Overlay) Anval ULTIMET is a cobalt-base alloy designed to be used as plasma transfer arc (PTA) overlay where corrosion aggravates wear. Anvai is a registered trademark of Anval Nyby Powder AB...
Journal Articles
Alloy Digest (1979) 28 (7): Co-23.
Published: 01 July 1979
... Molybdenum Tungsten Cobalt 0.90-1.40 Density, kg/cu m (At 22oC) 8387 2.00 max. lb/cu in. (At 72oF) 0.303 2.00 max. Melting range. oC (OF) 1265-1354 (2310-2470) 3.00 max. Specitic heat/of (At 720F) (Approx) 0.101 28.OG32.00 Thermal coef. expansion See Table 1 3.00 max. Thermal conductivity, Btu/ft2/in./hr...
Journal Articles
Alloy Digest (1984) 33 (5): SS-444.
Published: 01 May 1984
... is resistant to corrosion in hot chloride environments with low p H. It has good resistance to pitting and stress-corrosion cracking in chloride environments and is also resistant to oxidizing media. Its good resistance to corrosion has been demonstrated in both laboratory and field tests. These tests indicate...
Journal Articles
Alloy Digest (1974) 23 (3): Ni-46.
Published: 01 March 1974
...) 26.7 x 106 (At 1 600°F) 22.7 x 106 Magnetic permeability (H = 200 Oersteds) (Sol. treated + aged) 1.004 PROPERTIES Table 1 - THERMAL CONDUCTIVITY Table 2 - ELECTRICAL RESlSTlVlTY Temperature Btu/ft2/ Temperature Btu/ft2/ Condition Heat Treatment Ohms/cir mil ft OF hr/in./oF OF hr/inF A 19750F 4 hr. air...