Alloy Digest (1985) 34 (7): Ni-317.
Published: 01 July 1985
... HASTELLOY Alloy C-22 is a nickel-chromium-molybdenum alloy that has outstanding resistance to pitting, crevice corrosion and stress-corrosion cracking. The alloy also has excellent resistance to both reducing and oxidizing media. The alloy has good mechanical properties at both room and elevated...
Journal Articles
Alloy Digest (2019) 68 (5): Ni-752.
Published: 01 May 2019
... Hastelloy C-22 welding wire is used on Hastelloy alloy C-22, an excellent corrosion resistant material with exceptional diversity. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on joining. Filing Code: Ni-752. Producer...
Journal Articles
Alloy Digest (1985) 34 (9): Ni-322.
Published: 01 September 1985
... in phosphate rock source materials. In general. HASTELLOY ALLOY G-30 performs 2-10 times better than Alloy G or Alloy 625 in acids of intermediate corrosivity. In the annealed condition HASTELLOY ALLOY G-30 shows no loss in impact resistance at -320°F (-196°C). Forms Available: Plate, sheet, strip, billet, bar...
Journal Articles
Alloy Digest (2004) 53 (6): Ni-621.
Published: 01 June 2004
... ALLOY C-22HS (Corrosion-Resistant Nickel-Alloy) Hastelloy C-22HS has, like the other C-type alloys, excellent corrosion resistance, but it also exhibits high strength, nearly double the other alloys in the family. Hastelloy, C-22, and C-22HS are trademarks of Haynes International, Inc. 725...
Journal Articles
Alloy Digest (1993) 42 (8): Ni-440.
Published: 01 August 1993
... HASTELLOY alloy C-276 is a solid solution, nickel-molybdenum-chromium alloy, with outstanding resistance to localized corrosion and to both oxidizing and reducing media. (See Alloy Digest Ni-164, May 1971, for base metal.) This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1999) 48 (5): Ni-552.
Published: 01 May 1999
... periods of time. Postweld stress re- lieving near 650 °C (1200 °F) is not recommended. The only heat treatment that is recommended for alloy B-3 is a full solu- tion anneal at 1065 °C (1950 °F) for an appropriate time fol- lowed by a water quench or rapid air cool (depending on sec- tion thicknesses). 9...
Journal Articles
Alloy Digest (1994) 43 (9): Ni-464.
Published: 01 September 1994
...; NM64 - DIGEST- SEPTEMBER 1994 DATA ON WORLD WIDE METALS AND ALLOYS ocqyrigJy199d.mlyDk.AlllighLsnrserved p-by: AlbyDi Inc/201477-9161 Lmshmmprerypicpr.noftob8uredfor 27CanlieldStmel.Orarq.N.J.07050/U.SA speaiiicaba, Q hal c&s@. HASTELLOY@ D-20P ALLOY (Corrosion-resistant nickel-base alloy) HASTELLOY@ D...
Journal Articles
Alloy Digest (2004) 53 (7): Ni-622.
Published: 01 July 2004
... consists of heating at 1177 °C (2150 °F) and rapidly air cooling or water quenching. Hot-formed parts should be given this treatment prior to final fabrication or installation. Workability: This alloy can be fabricated using the same techniques as for Hastelloys G-3 and G-30. For detailed information...
Journal Articles
Alloy Digest (1988) 37 (12): Ni-365.
Published: 01 December 1988
.... It can be strength- ened only by cold work. The alloy may be solution treated at 2100°F (1 150°C) followed by rapid air cool or water quench. Machinability: HASTELLOY alloy H-9M machines similar to austenitic stainless steels. Use carbide or high-speed steel tools. Tools should be sharp, rigidly...
Journal Articles
Alloy Digest (1993) 42 (4): Ni-425.
Published: 01 April 1993
... cov- l ZLmpaatme range of 100@15oo F (S38-816OC) shonld be avoided. Postwdd stxess relieving in the UXPF (6Sm range will case embritdemmt and poMible necldag of the alloy. The only heat ueaenmt which is xccomnmdedforalloyB2isa fun solutial anneal at 195oT (1065 C) for an appr@aR tim followed...
Journal Articles
Alloy Digest (1985) 34 (8): Ni-320.
Published: 01 August 1985
... *Nominal compositions in 70: HAYNES 188: 40 Co, 22 Cr, 22 Ni and 14.5 W. HASTELLOY X: 49 Ni, 22 Cr, 9 MO, 15.8 Fe and 1.5 max. Co. Alloy HAYNES 230 HAYNES 188 HASTELLOY X *Test conditions: Metal Total Metal Affected Loss (Loss + max. pene- mils/ side tration) mils/ side 3.6 7.7 8.0 11.3 15.4 19.5 Burner...
Journal Articles
Alloy Digest (2015) 64 (12): SS-1234.
Published: 01 December 2015
... Chemical composition of welding materials for NSSMC-NAR-AC-3, AC-4 Welding consumables Ni Cr Mo Fe W Nb + Ta ASTM UNS No. Inconel 625 bal 22 9 <5 4 N06625 Hastelloy C-22 bal 22 13 4 3 N06022 Hastelloy C-276 bal 16 16 5 4 N10276 DOI: 10.31399/asm.ad.ss1234 ISSN: 002-614X SS-1234B Fig. 1 Electrode...
Journal Articles
Alloy Digest (1974) 23 (11): Ni-211.
Published: 01 November 1974
... HASTELLOY Alloy C-4 is a nickel-chromium-molybdenum alloy with outstanding high-temperature stability as shown by high ductility and corrosion resistance even after long-time aging in the range 1200-1900 F. Alloy C-4 also has excellent resistance to stress-corrosion cracking and to oxidizing...
Journal Articles
Alloy Digest (2018) 67 (3): Ni-742.
Published: 01 March 2018
... of Alloy Digest Ni-621. Hastelloy, C-22, and C-22HS are trademarks of Haynes International, Inc. Chemical Composition, wt.% (Nominal) Nickel (bal) Designation 61 Chromium 21 Molybdenum 17 Iron 2 max Tungsten 1 max Silicon 0.08 max Carbon 0.01 max Physical Properties Density, kg/m3 (lb/in.3) 8690 (0.323...
Journal Articles
Alloy Digest (2010) 59 (5): Ni-679.
Published: 01 May 2010
... rolled shells. No anneal is necessary for cold rolled vessel shells. Corrosion Resistance: This is a nickel alloy with superior resistance to hydrochloric and sulfuric acid while also having excellent sea and crevice corrosion. See Tables 3 and 4. Hastelloy, Hybrid-BC1, C-2000, and B3 are registered...
Journal Articles
Alloy Digest (1993) 42 (5): Ni-432.
Published: 01 May 1993
...* 0.50* Nickel Bal. Bal. *Maximum Physical Constants: Density, lb/cu in. (At 70°F) g/m cm (At 22 C) Thermal coef. expansion/ F (86400°F) (86-800°F) (8612OO F) PC (30~204°C) (30427°C) (30-649T) Thermal conductivity, Btu/ftz/in.ihr~F (At 75°F) (At 572= l=) (At 1112OF) WlmpC (At 24 C) (At 3OO C) (At 600°C...
Journal Articles
Alloy Digest (1954) 3 (12): Ni-14.
Published: 01 December 1954
... 35.0 444 61 G46 900 188.000 178.000 11.0 383 418 s6 c43 1000 17s.000 164,000 11.5 39.0 387 s3 c-39 1100 167.000 157.000 13.5 42.0 364 49 G37 1200 134,000 125. 00 18.0 52.0 302 43 c-32 800 209.000 188.000 10.0 900 188.000 174.000 11.5 1000 175,000 160.000 13.0 1100 164.000 152.000 15.5 1200 133.000...
Journal Articles
Alloy Digest (2005) 54 (3): Ni-624.
Published: 01 March 2005
.... Hastelloy and C-22 are trademarks of Haynes International, Inc. Nicrofer is a trademark of Thyssen Krupp VDM. Table 1 Typical Room Temperature Mechanical Properties of Inconel Alloy 22 Material thickness Tensile Yield strength, or diameter strength 0.2% offset Elongation, Hardness, Form mm in. MPa ksi MPa...
Journal Articles
Alloy Digest (2002) 51 (10): Ni-592.
Published: 01 October 2002
...) Yield strength, 0.2%, MPa (ksi) 252 (37) Elongation in 4d, % 44 Elongation in 5d, % 42 Impact toughness 196 °C 130 (96) ( 321 °F), J (ft lbf) Hardness, HV 220 Heat Treatment: The weld metal deposited from RIMA HAS C22 is normally used in the as-deposited condition. Weldability: Normally, no preheat...
Journal Articles
Alloy Digest (1993) 42 (7): Ni-437.
Published: 01 July 1993
... Alloy C-22 is a nickel-chromium-molybdenum alloy that has outstanding resistance to pitting, crevice corrosion and stress-corrosion cracking. The alloy also has excellent resistance to both reducing and oxidizing media. The alloy has good mechanical properties at both room and elevated...