Alloy Digest (1983) 32 (6): TS-414.
Published: 01 June 1983
... GUTERL S-7 is a chromium-molybdenum, general-purpose, air-hardening tool steel recommended for uses where shock resistance, good hot-work properties, good wear resistance, excellent toughness and easy machining are important. These properties make it suitable for many hot-work and cold-work...
Journal Articles
Alloy Digest (1982) 31 (3): TS-396.
Published: 01 March 1982
... GUTERL S-1 is a chromium-tungsten steel for general use for chisels and other cold-battering tools. It also is used for numerous other cold and hot-work applications because of its excellent toughness, high hardness and strength, and resistance to fatigue. Its many applications include...
Journal Articles
Alloy Digest (1979) 28 (12): TS-357.
Published: 01 December 1979
... GUTERL S-5 is a shock-resisting steel recommended for severe and repeated impacts in service. It has an excellent combination of toughness and hardness to survive the high stresses in service and to resist abrasion and wear. It is normally hardened by austenitizing and quenching in oil but it can...