Alloy Digest (1979) 28 (12): TS-357.
Published: 01 December 1979
... GUTERL S-5 is a shock-resisting steel recommended for severe and repeated impacts in service. It has an excellent combination of toughness and hardness to survive the high stresses in service and to resist abrasion and wear. It is normally hardened by austenitizing and quenching in oil but it can...
Journal Articles
Alloy Digest (1983) 32 (6): TS-414.
Published: 01 June 1983
... GUTERL S-7 is a chromium-molybdenum, general-purpose, air-hardening tool steel recommended for uses where shock resistance, good hot-work properties, good wear resistance, excellent toughness and easy machining are important. These properties make it suitable for many hot-work and cold-work...
Journal Articles
Alloy Digest (1981) 30 (12): TS-391.
Published: 01 December 1981
... GUTERL M-1 is a highly-molybdenum, low-tungsten type of high-speed tool steel. It is a general-purpose high-speed steel with an excellent combination of cutting ability, finishing characteristics and toughness. Guterl M-1 has good cutting ability for all operations except for heavy-duty...
Journal Articles
Alloy Digest (1979) 28 (5): TS-349.
Published: 01 May 1979
.... This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-349. Producer or source: Guterl Special Steel Corporation. Producer or Source: Guterl Special Steel Corporation Copyright © ASM...