1-1 of 1 Search Results for

GUTERL H-13

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1982) 31 (10): TS-405.
Published: 01 October 1982
... GUTERL H-13 is an air-hardening chromium-molybdenum-vanadium tool steel that finds wide use as dies in the forging, extrusions and die-casting industries. It has good hot hardness and wear resistance, extreme toughness and high resistance to heat checking and erosive action. Also, it has excellent...