Skip Nav Destination
Close Modal
Search Results for
GUTERL A-2
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-16 of 16 Search Results for
GUTERL A-2
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (6): TS-364.
Published: 01 June 1980
... GUTERL A-2 is a high-hardenability cold-work tool and die steel with excellent non-deforming properties. It is air hardening and therefore exhibits a high degree of dimensional stability in heat treatment. It is recommended where the application requires a good combination of machinability, wear...
Abstract
View article
PDF
GUTERL A-2 is a high-hardenability cold-work tool and die steel with excellent non-deforming properties. It is air hardening and therefore exhibits a high degree of dimensional stability in heat treatment. It is recommended where the application requires a good combination of machinability, wear resistance and toughness. Among the many uses of Guterl A-2 are shear blades, blanking and forming dies, punches and burnishing tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-364. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (4): TS-380.
Published: 01 April 1981
... GUTERL D-2 is a high-hardenability tool and die steel of the high-carbon, high-chromium type. It has high compressive strength, his resistance to abrasion, minimum distortion in hardening but only fair toughness. Among its many uses are rolls, punches, shear blades, lathe centers and many types...
Abstract
View article
PDF
GUTERL D-2 is a high-hardenability tool and die steel of the high-carbon, high-chromium type. It has high compressive strength, his resistance to abrasion, minimum distortion in hardening but only fair toughness. Among its many uses are rolls, punches, shear blades, lathe centers and many types of cutting and forming dies. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and surface treatment. Filing Code: TS-380. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (9): TS-387.
Published: 01 September 1981
... GUTERL M-2 is a molybdenum-tungsten type of high-speed steel with fairly good resistance to decarburization. It is a general-purpose high-speed steel and it provides excellent resistance to abrasion and shock. It is used widely for cutting tools. Among its many applications are hack saws, circular...
Abstract
View article
PDF
GUTERL M-2 is a molybdenum-tungsten type of high-speed steel with fairly good resistance to decarburization. It is a general-purpose high-speed steel and it provides excellent resistance to abrasion and shock. It is used widely for cutting tools. Among its many applications are hack saws, circular saws, lathe tools, gear cutters, planer tools and wood knives. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-387. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (8): TS-336.
Published: 01 August 1978
... SIMONDS D-2 is an air-hardening tool and die steel of the high-carbon, high-chromium type. It is characterized by high resistance to abrasion, fair toughness, minimum distortion in hardening and high compressive strength. Its many uses include a wide range of cutting and forming dies, rolls...
Abstract
View article
PDF
SIMONDS D-2 is an air-hardening tool and die steel of the high-carbon, high-chromium type. It is characterized by high resistance to abrasion, fair toughness, minimum distortion in hardening and high compressive strength. Its many uses include a wide range of cutting and forming dies, rolls, reamers, plug gages and shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-336. Producer or source: Guterl Special Steel Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (12): TS-343.
Published: 01 December 1978
... SIMONDS M-2 is a general-purpose high-speed steel with excellent resistance to abrasion and shock. It is a molybdenum-tungsten type of high-speed steel and is not particularly susceptible to decarburization. Its many applications include lathe tools, gear cutters, thread chasers and circular saws...
Abstract
View article
PDF
SIMONDS M-2 is a general-purpose high-speed steel with excellent resistance to abrasion and shock. It is a molybdenum-tungsten type of high-speed steel and is not particularly susceptible to decarburization. Its many applications include lathe tools, gear cutters, thread chasers and circular saws. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on high temperature performance as well as heat treating, machining, and joining. Filing Code: TS-343. Producer or source: Guterl Special Steel Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (6): TS-414.
Published: 01 June 1983
... 10 31 52 2 10000 10 33 51 195000 11 40 41 150000 14 48 38 130000 20 60 31 DOI: 10.31399/asm.ad.ts0414 Copyright © ASM International® 1996 Heat Treatment: Annealing: Heat Guterl S-7 slowly to 1500-155oOF. hold at temperature for I to II/i hours for each inch of greatest thickness. cool slowly...
Abstract
View article
PDF
GUTERL S-7 is a chromium-molybdenum, general-purpose, air-hardening tool steel recommended for uses where shock resistance, good hot-work properties, good wear resistance, excellent toughness and easy machining are important. These properties make it suitable for many hot-work and cold-work applications. Among its many uses are blanking dies, shear blades, punches and chisels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and surface treatment. Filing Code: TS-414. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (12): TS-391.
Published: 01 December 1981
... to abrasion and shock, (2) Good red hardness, (3) Lower density than that of AISI Type Tl high-speed steel, and (4) Hardening temperature lOOoF lower than that of AISI Type Tl. Guterl M-l is generally furnished in the annealed condi- tion so that it can be handled without difficulty in most machining...
Abstract
View article
PDF
GUTERL M-1 is a highly-molybdenum, low-tungsten type of high-speed tool steel. It is a general-purpose high-speed steel with an excellent combination of cutting ability, finishing characteristics and toughness. Guterl M-1 has good cutting ability for all operations except for heavy-duty, continuous cutting applications that require the ultimate in red hardness. Its toughness is as great as that of other high-speed steels. Its typical uses include circular saws, broaches, gear cutters, twist drills and taps. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-391. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (12): TS-357.
Published: 01 December 1979
... GUTERL S-5 is a shock-resisting steel recommended for severe and repeated impacts in service. It has an excellent combination of toughness and hardness to survive the high stresses in service and to resist abrasion and wear. It is normally hardened by austenitizing and quenching in oil but it can...
Abstract
View article
PDF
GUTERL S-5 is a shock-resisting steel recommended for severe and repeated impacts in service. It has an excellent combination of toughness and hardness to survive the high stresses in service and to resist abrasion and wear. It is normally hardened by austenitizing and quenching in oil but it can be water quenched successfully with proper precautions. Its many uses include hammers, hand chisels, boiler punches, shear blades and pneumatic tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-357. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (3): TS-412.
Published: 01 March 1983
... at 400°F per hour is 1460-1350°F. Annealing: The recommended annealing temperature for Guterl H- 1 I is 155@1650°F. The suggested practice is to use controlled-atmosphere furnaces. If 0.280 7.75 6.2x lO-6 6.5 x IO- 7. I x 1o-6 7.7 x 10-b 8.0 x IO+ 8.3 x IO+ 198 30x IO6 12 x .106 Table 2 -EFFECT...
Abstract
View article
PDF
GUTERL H-11 is a 5% chromium hot-work tool steel with an excellent combination of red hardness, shock resistance (toughness) and resistance to abrasion; these are the properties needed for good hot-work characteristics. It will withstand drastic cooling from maximum operating temperatures. Among the many uses for this steel are hot-die applications, structural parts for jet engines and missiles, extrusion mandrels and forging dies. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-412. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (4): TS-361.
Published: 01 April 1980
... in oil. Temper fairly soon after the part reaches a temperature near that of the cooling medium. Tempering: Guterl D-7 should be tempered in the range 300-1000°F to give a hardness of 65-58 Rockwell C. The tempering temperature should be adjusted to give the desired hardness (See Table 2) and to suit...
Abstract
View article
PDF
GUTERL D-7 is a high-carbon, high-chromium, high-vanadium tool and die steel. It is air hardening and therefore offers an extremely high degree of dimensional stability in heat treatment. In the hardened condition it has extremely high resistance to abrasion and wear. Its many applications include blanking and cold-drawing dies, punches, burnishing tools, slitter knives and gages. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating and machining. Filing Code: TS-361. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (9): TS-370.
Published: 01 September 1980
... GUTERL M-7 is a molybdenum type of high-speed steel. It is somewhat similar to AISI Type M1 tool steel but with higher percentages of carbon and vanadium to provide an improvement over M1 in cutting characteristics without a significant loss in toughness. It is used widely for cutting-tool...
Abstract
View article
PDF
GUTERL M-7 is a molybdenum type of high-speed steel. It is somewhat similar to AISI Type M1 tool steel but with higher percentages of carbon and vanadium to provide an improvement over M1 in cutting characteristics without a significant loss in toughness. It is used widely for cutting-tool applications that require improved resistance to abrasion. Its many uses include reamers, twist drills, taps, lathe tools, end mills and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-370. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (1): TS-409.
Published: 01 January 1983
... GUTERL T-1 is a general-purpose high-speed steel that is suitable for practically all high-speed applications. It is relatively easy to fabricate. This steel has been the standard of the industry for many years because of its excellent combination of cutting ability and toughness, ease of heat...
Abstract
View article
PDF
GUTERL T-1 is a general-purpose high-speed steel that is suitable for practically all high-speed applications. It is relatively easy to fabricate. This steel has been the standard of the industry for many years because of its excellent combination of cutting ability and toughness, ease of heat treatment and minimum tendency to decarburize. Its many uses include drills, taps, broaches, hobs, lathe and planer tools, milling cutters and wood-working tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-409. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (2): TS-377.
Published: 01 February 1981
...: Annealing: Heat Guterl O-l to 1400-1450oF, soak adequately to bring the steel to this temperature, cool slowly at a maximum rate of 400F per hour. The typical annealed hardness is 183-2 12 Brinell. The surface of the steel should be protected by heating in a controlled- atmosphere furnace, in a vacuum...
Abstract
View article
PDF
GUTERL 0-1 is a nondeforming, oil-hardening, general-purpose tool and die steel. It can be oil hardened safely even in complex sections and shapes. It has a good combination of hardeness, toughness and resistance to abrasion and wear. Its many applications include dies for numerous purposes, broaches, forming rolls, stamps and knurling tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-377. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (10): TS-405.
Published: 01 October 1982
... GUTERL H-13 is an air-hardening chromium-molybdenum-vanadium tool steel that finds wide use as dies in the forging, extrusions and die-casting industries. It has good hot hardness and wear resistance, extreme toughness and high resistance to heat checking and erosive action. Also, it has excellent...
Abstract
View article
PDF
GUTERL H-13 is an air-hardening chromium-molybdenum-vanadium tool steel that finds wide use as dies in the forging, extrusions and die-casting industries. It has good hot hardness and wear resistance, extreme toughness and high resistance to heat checking and erosive action. Also, it has excellent machinability in the annealed condition and relatively good freedom from distortion and scaling during heat treatment. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-405. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (3): TS-396.
Published: 01 March 1982
... GUTERL S-1 is a chromium-tungsten steel for general use for chisels and other cold-battering tools. It also is used for numerous other cold and hot-work applications because of its excellent toughness, high hardness and strength, and resistance to fatigue. Its many applications include...
Abstract
View article
PDF
GUTERL S-1 is a chromium-tungsten steel for general use for chisels and other cold-battering tools. It also is used for numerous other cold and hot-work applications because of its excellent toughness, high hardness and strength, and resistance to fatigue. Its many applications include boilermaker's tools, cold-battering hand and pneumatic tools, punches, shear blades and concrete drills and breakers. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-396. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (5): TS-349.
Published: 01 May 1979
.... This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-349. Producer or source: Guterl Special Steel Corporation. Producer or Source: Guterl Special Steel Corporation Copyright © ASM...
Abstract
View article
PDF
A7W is a high-carbon cold-work tool and die steel with high hardenability. It can be heat treated to very high hardness to provide excellent resistance to abrasion and wear. Its applications include liners for sand and shot blasting machines, extrusion dies for ceramics, punches and knives. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-349. Producer or source: Guterl Special Steel Corporation.