Alloy Digest (1990) 39 (6): Cp-8.
Published: 01 June 1990
... GRILON PMV-4H is a reinforced nylon 6 injection molding resin optimally stabilized against high temperatures and ultra violet radiation. This datasheet provides information on physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information...