Skip Nav Destination
Close Modal
Search Results for
Finkl Steel Durodi
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
Finkl Steel Durodi
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (3): TS-789.
Published: 01 March 2020
... Finkl Steel Durodi is a nickel-chromium-molybdenum-vanadium, alloy hot work tool steel that hardens deeply and uniformly to a high hardness that holds up exceedingly well under impact and thermal shock. It is designed to provide maximum abrasion and heat resistance over a full range of service...
Abstract
View article
PDF
Finkl Steel Durodi is a nickel-chromium-molybdenum-vanadium, alloy hot work tool steel that hardens deeply and uniformly to a high hardness that holds up exceedingly well under impact and thermal shock. It is designed to provide maximum abrasion and heat resistance over a full range of service temperatures normally encountered in forging applications. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on high temperature performance as well as forming, machining, and joining. Filing Code: TS-789. Producer or source: Finkl Steel (a Schmolz + Bickenbach Group company).
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1997) 46 (5): TS-555.
Published: 01 May 1997
... DURODI is a hot-work die steel with relatively high percentages of nickel, chromium, molybdenum, and silicon for good abrasion and heat resistance. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on heat treating and joining...
Abstract
View article
PDF
DURODI is a hot-work die steel with relatively high percentages of nickel, chromium, molybdenum, and silicon for good abrasion and heat resistance. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on heat treating and joining. Filing Code: TS-555. Producer or source: A. Finkl & Sons Company.