Skip Nav Destination
Close Modal
Search Results for
Fifth-Vickers F.V. 520(S)
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Fifth-Vickers F.V. 520(S)
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1968) 17 (4): SS-208.
Published: 01 April 1968
... Fifth-Vickers F.V. 520(S) is a corrosion resistant martensitic steel which is readily weldable and capable of being hardened by low temperature heat treatment. It is recommended for turbine components and supersonic aircraft parts. This datasheet provides information on composition, physical...
Abstract
View article
PDF
Fifth-Vickers F.V. 520(S) is a corrosion resistant martensitic steel which is readily weldable and capable of being hardened by low temperature heat treatment. It is recommended for turbine components and supersonic aircraft parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: SS-208. Producer or source: Firth-Vickers Stainless Steels Ltd.