Journal Articles
Alloy Digest (1964) 13 (3): TS-145.
Published: 01 March 1964
... Ferro-Tic J is a cemented carbide bonded with a modified high-speed steel. It is machinable and heat treatable. It is recommended for cutting tools. This datasheet provides information on composition and physical properties. It also includes information on heat treating, machining, and joining...