Alloy Digest (2013) 62 (1): SS-1133.
Published: 01 January 2013
... Ferralium 255-SD50 has much higher strength than other commercially available superduplex alloys. Ferralium 255 is the original superduplex stainless steel, noted for its unique combination of mechanical properties and resistance to corrosion, erosion, and cavitation. It has especially low...
Journal Articles
Alloy Digest (2007) 56 (7): Ni-653.
Published: 01 July 2007
... Comparisons Yield strength, min Corrosion rate, mm/yr Alloy MPa ksi Seawater 10% sulfuric acid at 80 °C (175 °F) 50% nitric acid, boiling N04400 170 25 0.25 0.06 1.1 S31803 450 65 <0.01 0.4 >5 718, aged 827 120 <0.01 <0.15 >1.5 N05500 690 100 0.18 0.1 <2 Ferralium 255-SD50 600 87 <0.01 <0.15 >5 Table 1 Basic...
Journal Articles
Alloy Digest (2012) 61 (12): SS-1129.
Published: 01 December 2012
... (0.06) < 0.4 (< 0.02) RC20 Ferralium 255-SD50 610 (88) < 0.01 (< 0.0004) < 0.15 (< 0.006) < 0.15 (< 0.006) RC27 ...
Journal Articles
Alloy Digest (2007) 56 (6): Ni-651.
Published: 01 June 2007
... Seawater 10% sulfuric acid at 80 °C (176 °F) Boiling 50% nitric acid N04400 170 25 0.25 0.06 1.1 S31803 450 65 <0.01 0.4 >5 718 (ST) 550 max 80 max <0.01 <0.15 >1.5 N05500 690 100 0.18 0.1 <2 Ferralium 255-SD50 600 87 <0.01 <0.15 >5 DOI: 10.31399/asm.ad.ni0651 even this concentration is too high except...