Alloy Digest (2007) 56 (1): SS-983.
Published: 01 January 2007
... Ferralium 255-FG46 is a cold work hardened fastener grade with a pitting resistance equivalent number (PREN) of 40 minimum. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes...