Alloy Digest (1956) 5 (7): Sn-2.
Published: 01 July 1956
...: Federated Metals Corporation, ASARCO Inc. Copyright © ASM International® 1996 1996 ASM International castability chemical composition compressive strength elasticity fatigue properties Federated no. 3 frictional resistance hardness joinability physical properties tensile properties...
Journal Articles
Alloy Digest (1956) 5 (8): Pb-3.
Published: 01 August 1956
... properties as well as fatigue. It also includes information on casting and joining. Filing Code: Pb-3. Producer or source: Federated Metals Corporation, ASARCO Inc.. Producer or Source: Federated Metals Corporation, ASARCO Inc. Copyright © ASM International® 1996 1996 ASM International...
Journal Articles
Alloy Digest (1956) 5 (6): Zn-3.
Published: 01 June 1956
..., physical properties, hardness, tensile properties, and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Zn-3. Producer or source: Federated Metals Corporation, ASARCO Inc...
Journal Articles
Alloy Digest (1973) 22 (7): Pb-11.
Published: 01 July 1973
... G Babbit is a lead-base bearing alloy high in arsenic (2.5-3%) for high loads and speeds. It was designed to provide relatively high strength and hardness, especially at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1990) 39 (8): CI-62.
Published: 01 August 1990
... Ductile Dura-Bar has somewhat greater tensile strength up to 3 diameter and considerably higher yield strength up through 10 diameter. The elongation of 70-02 is lower than that of 55-06 because of its reduced ferrite content. This datasheet provides information on composition, microstructure...
Journal Articles
Alloy Digest (1975) 24 (11): Al-219.
Published: 01 November 1975
... FEDERATED F150.5 is a heat-treatable aluminum alloy containing silicon and copper as the major alloying elements. It is recommended for high-strength, light-weight, pressure-tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1975) 24 (2): Al-213.
Published: 01 February 1975
... FEDERATED F450 is a heat-treatable sand and permanent-mold aluminum casting alloy with good casting characteristics and pressure tightness. It is recommended for general-purpose castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1974) 23 (10): Al-209.
Published: 01 October 1974
... Federated F070.3 is a heat-treatable aluminum casting alloy recommended for high strength, good corrosion resistance, pressue-tight castings and intricate shapes. It is normally used only when heat-treated (aged) strengths are required. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1974) 23 (11): Al-210.
Published: 01 November 1974
... FEDERATED F410 is a heat-treatable aluminum sand casting alloy recommended for uses requiring high strength along with toughness and ductility. It has good machinability, fair castability, and is suitable for a number of automotive and aerospace applications. This datasheet provides information...
Journal Articles
Alloy Digest (1977) 26 (5): Al-226.
Published: 01 May 1977
..., and air cool. Solution Treatment - Aging: Heat to 950oF, hold at temperature 6-12 hours, quench in hot water at 180-2120F (Boiling water is desired to minimize distor- tion and cracking), age at 3100F for 3-16 hours, air cool. Machinability: Federated F41_10 has only a fair machinability rating; however...
Journal Articles
Alloy Digest (1977) 26 (1): Al-118.
Published: 01 January 1977
... FEDERATED F430 is a heat-treatable aluminum-copper-silicon casting alloy with good castability, machinability and corrosion resistance. It is produced by sand casting and is a general-purpose alloy recommended in both the as-cast and heat-treated conditions. This datasheet provides information...
Journal Articles
Alloy Digest (1974) 23 (12): Al-212.
Published: 01 December 1974
... quenching stresses and distortion. Age at 4OOoF for 3-5 hours, air cool. (Permanent mold castings) Solution Treat + Overage to Stabilize (T77 Temper): Heat to 96OoF, hold 6 hours at temperature, air cool, overage at 6500F for 1-3 hours. (Sand castings). Machinability: Federated F401.5Ni has good...
Journal Articles
Alloy Digest (1968) 17 (10): Al-180.
Published: 01 October 1968
... FEDERATED F460 is a heat treatable, aluminum-base, sand and permanent mold casting alloy having good foundry characteristics and pressure tightness. It is recommended for general purpose castings in either the as-cast or heat treated condition. The F460PT grade is specially processed during...
Journal Articles
Alloy Digest (1958) 7 (7): Pb-5.
Published: 01 July 1958
... Federated No. 15 is a lead-base alloy having high fatigue resistance. It is recommended for good service in precision bearings. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength as well as fracture toughness and fatigue...
Journal Articles
Alloy Digest (1957) 6 (11): Pb-4.
Published: 01 November 1957
... FEDERATED No. 14 is a lead-base bearing alloy having superior fatigue resistance. It is decommended for excellent service in precision bearings. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength as well as fracture...
Journal Articles
Alloy Digest (1976) 25 (12): Cu-324.
Published: 01 December 1976
.... It is characterized by unusual resistance to wear. The outstanding merits claimed for Federal Bronze 822 can be summarized as followes: (1) Non seizing and non-scoring, (2) Long wearing, (3) Self lubricating, (4) Low coefficient of friction, (5) High compressive strength, (6) Good resistance to shock loading, (7...
Journal Articles
Alloy Digest (1962) 11 (5): Al-114.
Published: 01 May 1962
... Federated F050 is a 5% silicon-aluminum casting alloy recommended for intricate design and thin wall castings. It produces pressure tight castings and has a high resistance to corrosion. The F050 PT grade is specially processed during manufacture to reduce the apparent solidification shrinkage...
Journal Articles
Alloy Digest (1976) 25 (2): Al-221.
Published: 01 February 1976
... FEDERATED F0120 is a high-silicon aluminum alloy suitable for sand, permanent-mold and die casting. It is used for intricate thin-walled castings requiring pressure tightness, toughness and good resistance to corrosion. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1977) 26 (7): Al-227.
Published: 01 July 1977
... FEDERATED F024 is an aluminum sand casting alloy characterized by moderate strength, good pressure tightness and excellent resistance to corrosion and staining. Its uses include such items as marine hardware and cooking utensils. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1977) 26 (3): Al-225.
Published: 01 March 1977
... FEDERATED F1121 Ni is a heat-treatable aluminum-silicon-nickel-copper-magnesium alloy used for high-strength permanent-mold castings. It can be solution treated and aged, or the as-cast material can be aged to increase hardness and strength. Its uses include pistons and pulleys. This datasheet...