Skip Nav Destination
Close Modal
Search Results for
Federated no. 2
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 414
Search Results for Federated no. 2
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
FEDERATED No. 2: Bearing Alloy
Available to Purchase
Alloy Digest (1954) 3 (10): Sn-1.
Published: 01 October 1954
... Federated No. 2 is a tin-base white Babbitt metal used for bearings where speeds, loads and stresses are moderate to high. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> No. <span class="search-highlight">2</span>: Bearing Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> No. <span class="search-highlight">2</span>: Bearing Alloy
Federated No. 2 is a tin-base white Babbitt metal used for bearings where speeds, loads and stresses are moderate to high. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on casting and joining. Filing Code: Sn-1. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED No. 3: Tin-Base Bearing Alloy
Available to Purchase
Alloy Digest (1956) 5 (7): Sn-2.
Published: 01 July 1956
... provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on casting and joining. Filing Code: Sn-2. Producer or source: Federated Metals Corporation, ASARCO Inc.. Producer or Source...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> No. 3: Tin-Base Bearing Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> No. 3: Tin-Base Bearing Alloy
FEDRATED NO. 3 is a tin-base bearing alloy recommended for moderate to high speeds and loads. It has low frictional resistance, low wear, good running-in properties, good emergency behavior upon failing of lubrication, and lower coefficient of expension than the lead-base alloys. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on casting and joining. Filing Code: Sn-2. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
CONTINUOUS-CAST GRAY IRONS: Continuous Cast Gray Irons, Types G1 and G2
Available to Purchase
Alloy Digest (1989) 38 (2): CI-57.
Published: 01 February 1989
... Types G-1 and G-2 gray iron bar and plate produced by continuous casting have consistent density and hardness with improved toughness, providing greater durability and more dependable performance than conventionally cast grades. This datasheet provides information on composition, physical...
Abstract
View articletitled, CONTINUOUS-CAST GRAY IRONS: Continuous Cast Gray Irons, Types G1 and G2
View
PDF
for article titled, CONTINUOUS-CAST GRAY IRONS: Continuous Cast Gray Irons, Types G1 and G2
Types G-1 and G-2 gray iron bar and plate produced by continuous casting have consistent density and hardness with improved toughness, providing greater durability and more dependable performance than conventionally cast grades. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on heat treating and machining. Filing Code: CI-57. Producer or source: Federal Bronze Products Inc..
Journal Articles
ASARCOLO 158-190 and 217-440: Bismuth-Base Fusible Alloys
Available to Purchase
Alloy Digest (1978) 27 (1): Bi-2.
Published: 01 January 1978
... information on forming, heat treating, machining, and joining. Filing Code: Bi-2. Producer or source: Federated Metals Corporation, ASARCO Inc.. Producer or Source: Federated Metals Corporation, ASARCO Inc. Copyright © ASM International® 1996 1996 ASM International anchoring components ASARCOLO...
Abstract
View articletitled, ASARCOLO 158-190 and 217-440: Bismuth-Base Fusible Alloys
View
PDF
for article titled, ASARCOLO 158-190 and 217-440: Bismuth-Base Fusible Alloys
ASARCOLO 158-190 and 217-440 are non-eutectic alloys that can be melted easily. Each range indicates the range through which the alloy melts; thus ASARCOLO 158-190 is a non-eutectic alloy that has a melting range from 158 F to 190 F and ASARCOLO 217-440 is another non-eutectic alloy that melts in the range 217 F to 440 F. These alloys are used widely to aid foundry and machine shop practices, for anchoring components, to spot fixtures for awkward shapes, and for soldering. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Bi-2. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED F4110: Aluminum Casting Alloy
Available to Purchase
Alloy Digest (1977) 26 (5): Al-226.
Published: 01 May 1977
... FEDERATED F4110 is a general-purpose alloy for making intricate die castings. It is also used for thin-walled, complicated permanent-mold castings where maximum fluidity, pressure tightness and resistance to hot cracking are required. It has excellent castability and foundry characteristics, fair...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> F4110: Aluminum Casting Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> F4110: Aluminum Casting Alloy
FEDERATED F4110 is a general-purpose alloy for making intricate die castings. It is also used for thin-walled, complicated permanent-mold castings where maximum fluidity, pressure tightness and resistance to hot cracking are required. It has excellent castability and foundry characteristics, fair machinability and good strength. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-226. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED F070.3: Heat Treatable Aluminum Casting Alloy
Available to Purchase
Alloy Digest (1974) 23 (10): Al-209.
Published: 01 October 1974
... Federated F070.3 is a heat-treatable aluminum casting alloy recommended for high strength, good corrosion resistance, pressue-tight castings and intricate shapes. It is normally used only when heat-treated (aged) strengths are required. This datasheet provides information on composition, physical...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> F070.3: Heat Treatable Aluminum Casting Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> F070.3: Heat Treatable Aluminum Casting Alloy
Federated F070.3 is a heat-treatable aluminum casting alloy recommended for high strength, good corrosion resistance, pressue-tight castings and intricate shapes. It is normally used only when heat-treated (aged) strengths are required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-209. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED No. 15: Lead-Base Bearing Alloy
Available to Purchase
Alloy Digest (1958) 7 (7): Pb-5.
Published: 01 July 1958
... Federated No. 15 is a lead-base alloy having high fatigue resistance. It is recommended for good service in precision bearings. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength as well as fracture toughness and fatigue...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> No. 15: Lead-Base Bearing Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> No. 15: Lead-Base Bearing Alloy
Federated No. 15 is a lead-base alloy having high fatigue resistance. It is recommended for good service in precision bearings. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on casting and joining. Filing Code: Pb-5. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED F150.5: Heat Treatable Aluminum Casting Alloy
Available to Purchase
Alloy Digest (1975) 24 (11): Al-219.
Published: 01 November 1975
... FEDERATED F150.5 is a heat-treatable aluminum alloy containing silicon and copper as the major alloying elements. It is recommended for high-strength, light-weight, pressure-tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> F150.5: Heat Treatable Aluminum Casting Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> F150.5: Heat Treatable Aluminum Casting Alloy
FEDERATED F150.5 is a heat-treatable aluminum alloy containing silicon and copper as the major alloying elements. It is recommended for high-strength, light-weight, pressure-tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as casting, heat treating, machining, and joining. Filing Code: Al-219. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED F024: Aluminum Casting Alloy
Available to Purchase
Alloy Digest (1977) 26 (7): Al-227.
Published: 01 July 1977
... (500.kgf, 1 O-mm) 60 Compressive yield strength, psi 14000 Shear strength, psi 17000 Table 2 - MECHANICAL PROPERTY LIMITS (Separately sand cast specimens in as-cast condition, F temper) (As specified in ASTM B 26 for Aluminum B514.0 which is Federated F024) Tensile strength, mm, psi 17000 Yield...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> F024: Aluminum Casting Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> F024: Aluminum Casting Alloy
FEDERATED F024 is an aluminum sand casting alloy characterized by moderate strength, good pressure tightness and excellent resistance to corrosion and staining. Its uses include such items as marine hardware and cooking utensils. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength. It also includes information on corrosion resistance as well as casting, heat treating, and machining. Filing Code: Al-227. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED F450: Aluminum Casting Alloy
Available to Purchase
Alloy Digest (1975) 24 (2): Al-213.
Published: 01 February 1975
... FEDERATED F450 is a heat-treatable sand and permanent-mold aluminum casting alloy with good casting characteristics and pressure tightness. It is recommended for general-purpose castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> F450: Aluminum Casting Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> F450: Aluminum Casting Alloy
FEDERATED F450 is a heat-treatable sand and permanent-mold aluminum casting alloy with good casting characteristics and pressure tightness. It is recommended for general-purpose castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-213. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED No. 14: Lead-Base Bearing Alloy
Available to Purchase
Alloy Digest (1957) 6 (11): Pb-4.
Published: 01 November 1957
... FEDERATED No. 14 is a lead-base bearing alloy having superior fatigue resistance. It is decommended for excellent service in precision bearings. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength as well as fracture...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> No. 14: Lead-Base Bearing Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> No. 14: Lead-Base Bearing Alloy
FEDERATED No. 14 is a lead-base bearing alloy having superior fatigue resistance. It is decommended for excellent service in precision bearings. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on casting and joining. Filing Code: Pb-4. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED F0120: Aluminum Casting Alloy
Available to Purchase
Alloy Digest (1976) 25 (2): Al-221.
Published: 01 February 1976
... temperatures) Test Tensile Yield Strength Temperature Strength (0.2% Offset) oF psi psi Elongation (2-in.) c ; C 212 34000 21000 5 300 30000 19000 8 400 24000 15000 15 500 13000 9000 30 Copyright © ASM International® 1996DOI: 10.31399/asm.ad.al0221 Heat Treatment: Federated FOG0 alloy is used normally...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> F0120: Aluminum Casting Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> F0120: Aluminum Casting Alloy
FEDERATED F0120 is a high-silicon aluminum alloy suitable for sand, permanent-mold and die casting. It is used for intricate thin-walled castings requiring pressure tightness, toughness and good resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-221. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED F430: Heat Treatable Aluminum Casting Alloy
Available to Purchase
Alloy Digest (1977) 26 (1): Al-118.
Published: 01 January 1977
... FEDERATED F430 is a heat-treatable aluminum-copper-silicon casting alloy with good castability, machinability and corrosion resistance. It is produced by sand casting and is a general-purpose alloy recommended in both the as-cast and heat-treated conditions. This datasheet provides information...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> F430: Heat Treatable Aluminum Casting Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> F430: Heat Treatable Aluminum Casting Alloy
FEDERATED F430 is a heat-treatable aluminum-copper-silicon casting alloy with good castability, machinability and corrosion resistance. It is produced by sand casting and is a general-purpose alloy recommended in both the as-cast and heat-treated conditions. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-118. Producer or source: Federated Metals Corporation, ASARCO Inc.. Originally published September 1962, revised January 1977.
Journal Articles
FEDERATED F401.5Ni: Heat Treatable Aluminum Alloy
Available to Purchase
Alloy Digest (1974) 23 (12): Al-212.
Published: 01 December 1974
... FEDERATED F401.5Ni is a heat-treatable aluminum casting alloy with high strength and good wear resistance in the fully heat-treated condition. It is recommended for castings requiring good strength at elevated temperatures. This datasheet provides information on composition, physical properties...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> F401.5Ni: Heat Treatable Aluminum Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> F401.5Ni: Heat Treatable Aluminum Alloy
FEDERATED F401.5Ni is a heat-treatable aluminum casting alloy with high strength and good wear resistance in the fully heat-treated condition. It is recommended for castings requiring good strength at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-212. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED F410: Heat Treatable Aluminum Casting Alloy
Available to Purchase
Alloy Digest (1974) 23 (11): Al-210.
Published: 01 November 1974
... FEDERATED F410 is a heat-treatable aluminum sand casting alloy recommended for uses requiring high strength along with toughness and ductility. It has good machinability, fair castability, and is suitable for a number of automotive and aerospace applications. This datasheet provides information...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> F410: Heat Treatable Aluminum Casting Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> F410: Heat Treatable Aluminum Casting Alloy
FEDERATED F410 is a heat-treatable aluminum sand casting alloy recommended for uses requiring high strength along with toughness and ductility. It has good machinability, fair castability, and is suitable for a number of automotive and aerospace applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-210. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED F1121Ni: Heat Treatable Aluminum Casting Alloy
Available to Purchase
Alloy Digest (1977) 26 (3): Al-225.
Published: 01 March 1977
... FEDERATED F1121 Ni is a heat-treatable aluminum-silicon-nickel-copper-magnesium alloy used for high-strength permanent-mold castings. It can be solution treated and aged, or the as-cast material can be aged to increase hardness and strength. Its uses include pistons and pulleys. This datasheet...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> F1121Ni: Heat Treatable Aluminum Casting Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> F1121Ni: Heat Treatable Aluminum Casting Alloy
FEDERATED F1121 Ni is a heat-treatable aluminum-silicon-nickel-copper-magnesium alloy used for high-strength permanent-mold castings. It can be solution treated and aged, or the as-cast material can be aged to increase hardness and strength. Its uses include pistons and pulleys. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-225. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERAL BRONZE 822: High Leaded Tin Bronze
Available to Purchase
Alloy Digest (1976) 25 (12): Cu-324.
Published: 01 December 1976
.... It is characterized by unusual resistance to wear. The outstanding merits claimed for Federal Bronze 822 can be summarized as followes: (1) Non seizing and non-scoring, (2) Long wearing, (3) Self lubricating, (4) Low coefficient of friction, (5) High compressive strength, (6) Good resistance to shock loading, (7...
Abstract
View articletitled, <span class="search-highlight">FEDERAL</span> BRONZE 822: High Leaded Tin Bronze
View
PDF
for article titled, <span class="search-highlight">FEDERAL</span> BRONZE 822: High Leaded Tin Bronze
FEDERAL BRONZE 822 is a copper-base, high-lead bearing bronze with superior resistance to scoring and seizure beyond the endurance and danger limits of ordinary bearing bronzes. It is used in applications involving high speeds, poor lubrication, heat-generating loads, elevated temperatures, dusty and gritty surroundings, or where a liquid other than oil is used as the lubricant. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on casting, heat treating, machining, joining, and surface treatment. Filing Code: Cu-324. Producer or source: Federal Bronze Products Inc..
Journal Articles
FEDERATED F460: General Purpose Casting Alloy
Available to Purchase
Alloy Digest (1968) 17 (10): Al-180.
Published: 01 October 1968
... FEDERATED F460 is a heat treatable, aluminum-base, sand and permanent mold casting alloy having good foundry characteristics and pressure tightness. It is recommended for general purpose castings in either the as-cast or heat treated condition. The F460PT grade is specially processed during...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> F460: General Purpose Casting Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> F460: General Purpose Casting Alloy
FEDERATED F460 is a heat treatable, aluminum-base, sand and permanent mold casting alloy having good foundry characteristics and pressure tightness. It is recommended for general purpose castings in either the as-cast or heat treated condition. The F460PT grade is specially processed during manufacture to reduce the apparent solidification shrinkage with no change in chemical specification or mechanical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-180. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED No. 8: Lead-Base Bearing Alloy
Available to Purchase
Alloy Digest (1956) 5 (8): Pb-3.
Published: 01 August 1956
... FEDERATED No. 8 is a lead-base bearing alloy recommended for moderate to high speeds and moderate loads. It has very good frictional properties, reasonably good corrosion resistance and low price. This datasheet provides information on composition, physical properties, hardness, and tensile...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> No. 8: Lead-Base Bearing Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> No. 8: Lead-Base Bearing Alloy
FEDERATED No. 8 is a lead-base bearing alloy recommended for moderate to high speeds and moderate loads. It has very good frictional properties, reasonably good corrosion resistance and low price. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fatigue. It also includes information on casting and joining. Filing Code: Pb-3. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED F050 and F050PT: Aluminum Casting Alloy
Available to Purchase
Alloy Digest (1962) 11 (5): Al-114.
Published: 01 May 1962
... Federated F050 is a 5% silicon-aluminum casting alloy recommended for intricate design and thin wall castings. It produces pressure tight castings and has a high resistance to corrosion. The F050 PT grade is specially processed during manufacture to reduce the apparent solidification shrinkage...
Abstract
View articletitled, <span class="search-highlight">FEDERATED</span> F050 and F050PT: Aluminum Casting Alloy
View
PDF
for article titled, <span class="search-highlight">FEDERATED</span> F050 and F050PT: Aluminum Casting Alloy
Federated F050 is a 5% silicon-aluminum casting alloy recommended for intricate design and thin wall castings. It produces pressure tight castings and has a high resistance to corrosion. The F050 PT grade is specially processed during manufacture to reduce the apparent solidification shrinkage with no change in the chemical specification or mechanical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-114. Producer or source: Federated Metals Corporation, ASARCO Inc..