1-1 of 1 Search Results for

Federalloy I-836

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1997) 46 (4): Cu-612.
Published: 01 April 1997
... Federalloy I-836 (C89833) is a lead-free bronze casting alloy that is machinable by alloying additions of bismuth. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also...