Alloy Digest (1954) 3 (1): W-1.
Published: 01 January 1954
... FANSTEEL 77 METAL is a sintered high density alloy made by powder metallurgy methods for use as an inertial mass for gyroscope rotors, as a counterbalance material, as a radiation shield, and the like. This datasheet provides information on composition, physical properties, hardness, elasticity...