Alloy Digest (1968) 17 (2): TS-202.
Published: 01 February 1968
... FAGERSTA-D66 is a 9% tungsten type hot-work tool and die steel having excellent combination of abrasion resistance, red-hardness and toughness at high operating temperatures. It is recommended for hot extrusion and forming dies, punches, rivet sets, shear blades, etc. This datasheet provides...