Journal Articles
Alloy Digest (1977) 26 (3): CS-67.
Published: 01 March 1977
... FROSTLINE is a fine-grain, columbium-treated carbon steel designed to be an economical solution to structural design requirements at cold temperatures. Available in plate thicknesses up to 6 inches, it offers high levels of toughness at temperatures to 80 F and higher strength levels than...