Alloy Digest (1994) 43 (7): SS-569.
Published: 01 July 1994
... FORONI AF 918 is a superduplex stainless steel with 25 chromium and a PRE of 41 min. The alloy is a joint development with Dalmine S.p.A. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on low...