Alloy Digest (1999) 48 (11): TS-569.
Published: 01 November 1999
... Finkl ShelleX is a high-quality steel alloy melted, vacuum arc degassed, and forged. The alloy is similar to Shelldie (see Alloy Digest TS-554, April 1997) but has nearly twice the molybdenum content for excellent wear resistance under conditions of high die operating temperatures. The alloy...