Alloy Digest (1999) 48 (12): Al-364.
Published: 01 December 1999
... Finkl Alu-C is a modification of UNS A92618 with higher thermal conductivity and higher yield strength above 121 C (250 F) than aluminum alloy 7075-T651. Alu-C is used for general, low-volume plastic injection molds. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (10): Al-363.
Published: 01 October 1999
...) Electrical conductivity at 20 °C (68 °F), %IACS 37 Poisson s ratio at 20 °C (68 °F) 0.33 (a)Finkl Alu-X has higher thermal conductivity than many aluminum alloys used for tool and molds (12% higher than 7075-T651). The higher conductivity allows for faster cycle times due to the greater heat extraction...