Alloy Digest (1993) 42 (4): Fe-99.
Published: 01 April 1993
... Ferroperm is a soft magnetic alloy that contains 1% aluminum. This addition of aluminum combined with high-temperature annealing increases permeability and reduces coercivity without decreasing the high-saturation magnetization of pure iron. This datasheet provides information on composition...