Alloy Digest (1974) 23 (8): Ni-207.
Published: 01 August 1974
... FERRO-TIC HT-6 is comprised of a dispersion of extremely hard, inert titanium carbide grains in a precipitation-hardenable, nickel-base matrix. It provides a combination of oxidation, corrosion and wear resistance unavailable in other materials for tools and many other uses. This datasheet...
Journal Articles
Alloy Digest (1975) 24 (12): SS-322.
Published: 01 December 1975
... FERRO-TIC HT-2 is a dispersion of extremely hard titanium carbide grains in an austenitic, heat-resistant, age-hardenable, iron-nickel-chromium alloy matrix. It exhibits good strength and good resistance to oxidation, corrosion, carburization and wear up to 1350 F. This datasheet provides...