Alloy Digest (1987) 36 (1): SS-481.
Published: 01 January 1987
... FERRALIUM Alloy 255 is a high-strength super stainless steel. It combines high mechanical strength, ductility and hardness with excellent resistance to corrosion and erosion. Under most conditions of service, its corrosion resistance is superior to that of the fully austenitic AISI Types 304, 316...
Journal Articles
Alloy Digest (1995) 44 (8): SS-606.
Published: 01 August 1995
... FERRALIUM alloy 255-3SC are castings with an improved chemistry range compared with FERRALIUM alloy 255 (Alloy Digest SS-481, January 1987). The alloy has improved corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1995) 44 (9): SS-611.
Published: 01 September 1995
... FERRALIUM alloy SD40 is a modification of FERRALIUM alloy 255 (Alloy Digest SS-481, January 1987) with higher nominal molybdenum and nitrogen. It meets the empirical PREN formula to a minimum 40. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2008) 57 (2): SS-1007.
Published: 01 February 2008
... Ferralium 255-3AF is a modification of Ferralium 255 (see Alloy Digest SS-481, January 1987), one of the early superduplex stainless steels. The 255 alloy has been modified over time with special chemistry, heat treatment, and production methods. This version is the age-hardened grade...
Journal Articles
Alloy Digest (2008) 57 (4): SS-1010.
Published: 01 April 2008
... Ferralium 255-3SF is an austenitic/ferritic duplex stainless steel equivalent to UNS S32550 as a forged product in bars, discs, and blocks. See also Ferralium 255, Alloy Digest SS-481, January 1987. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2013) 62 (1): SS-1133.
Published: 01 January 2013
... Ferralium 255-SD50 has much higher strength than other commercially available superduplex alloys. Ferralium 255 is the original superduplex stainless steel, noted for its unique combination of mechanical properties and resistance to corrosion, erosion, and cavitation. It has especially low...
Journal Articles
Alloy Digest (2007) 56 (1): SS-983.
Published: 01 January 2007
... information on corrosion resistance as well as forming and machining. Filing Code: SS-983. Producer or source: Langley Alloys. Producer or Source: Langley Alloys Copyright © ASM International® 2007 2007 ASM International chemical composition corrosion-resistant alloys elasticity Ferralium 255...
Journal Articles
Alloy Digest (1995) 44 (7): Cu-602.
Published: 01 July 1995
... cupronickel coupled with FERRALIUM alloy 255, have shown no enhanced attack on the cupronickel under the crevice conditions applied. When dissimilar metals are present, good design usually minimizes the danger of galvanic corro- sion by ensuring the more noble components (cathodic) are of smaller surface area...
Journal Articles
Alloy Digest (2007) 56 (8): SS-995.
Published: 01 August 2007
... S32550 (wrought) ASTM A 351 and A 744 grade CD4MCu(N) ASTM A890 grade 1A, UNS J93370 ASTM A 890 grade 1B, UNS J93372 BS 3100, grade 332C13 BS 3146, grade ANC21 DIN 1.4515, G-X3CrNiMoCuN 26 6 3 DIN 1.4517, G-X3CrNiMoCuN 26 6 3 3 Proprietary alloys Ferralium 255 and SD40 (Meighs); Uranus 50M, 55, 52N, 52N...
Journal Articles
Alloy Digest (2007) 56 (7): Ni-653.
Published: 01 July 2007
... Comparisons Yield strength, min Corrosion rate, mm/yr Alloy MPa ksi Seawater 10% sulfuric acid at 80 °C (175 °F) 50% nitric acid, boiling N04400 170 25 0.25 0.06 1.1 S31803 450 65 <0.01 0.4 >5 718, aged 827 120 <0.01 <0.15 >1.5 N05500 690 100 0.18 0.1 <2 Ferralium 255-SD50 600 87 <0.01 <0.15 >5 Table 1 Basic...
Journal Articles
Alloy Digest (2012) 61 (12): SS-1129.
Published: 01 December 2012
... (0.06) < 0.4 (< 0.02) RC20 Ferralium 255-SD50 610 (88) < 0.01 (< 0.0004) < 0.15 (< 0.006) < 0.15 (< 0.006) RC27 ...
Journal Articles
Alloy Digest (2007) 56 (6): Ni-651.
Published: 01 June 2007
... Seawater 10% sulfuric acid at 80 °C (176 °F) Boiling 50% nitric acid N04400 170 25 0.25 0.06 1.1 S31803 450 65 <0.01 0.4 >5 718 (ST) 550 max 80 max <0.01 <0.15 >1.5 N05500 690 100 0.18 0.1 <2 Ferralium 255-SD50 600 87 <0.01 <0.15 >5 DOI: 10.31399/asm.ad.ni0651 even this concentration is too high except...