Alloy Digest (2008) 57 (2): SS-1007.
Published: 01 February 2008
... Ferralium 255-3AF is a modification of Ferralium 255 (see Alloy Digest SS-481, January 1987), one of the early superduplex stainless steels. The 255 alloy has been modified over time with special chemistry, heat treatment, and production methods. This version is the age-hardened grade...