Alloy Digest (1977) 26 (5): Al-226.
Published: 01 May 1977
... FEDERATED F4110 is a general-purpose alloy for making intricate die castings. It is also used for thin-walled, complicated permanent-mold castings where maximum fluidity, pressure tightness and resistance to hot cracking are required. It has excellent castability and foundry characteristics, fair...