Alloy Digest (2006) 55 (8): CI-63.
Published: 01 August 2006
... F15-3 A, F15-3 B, and F15-3 C are abrasion-resistant cast alloys with varying combinations of elements to offer different levels of abrasion resistance and toughness. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength...
Journal Articles
Alloy Digest (1989) 38 (11): SS-204.
Published: 01 November 1989
... Tensile strength, ksi 190 170 0.2% Yield strength, ksi 170 155 Elongation (2 in. or 4D). % 10.0 10.0 6.0 7.0 Reduction of area, % 35.0 38.0 15.0 20.0 Hardness, Rockwell C 40147 38145 Charpy V-Notch impact, ft-lb # 5 # # HlO25 155 145 12.0 8.0 45.0 27.0 35142 15 10 H 1075 145 125 13.0 9.0 45.0 3%: 20 15...