1-1 of 1 Search Results for

F15-3 B

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2006) 55 (8): CI-63.
Published: 01 August 2006
... F15-3 A, F15-3 B, and F15-3 C are abrasion-resistant cast alloys with varying combinations of elements to offer different levels of abrasion resistance and toughness. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength...