Alloy Digest (1966) 15 (2): Cu-161.
Published: 01 February 1966
... EVERDUR-655 is a copper-silicon-manganese alloy having the desired combination of high strength, good workability, weldability and machinability along with high corrosion resistance. It is recommended for fasteners, springs pressure vessels and general hardware. This datasheet provides information...
Journal Articles
Alloy Digest (1970) 19 (3): Cu-213.
Published: 01 March 1970
..., spot resistance and butt resistance welding will produce good results, with only fair results obtained by oxyacetylene.carbon-arc, gas shielded arc, and seam resistance welding. Coated metal arc welding is not recommended: Ambraloy 687 tubes are successfully joined to Everdur 655 tube sheets with...