Alloy Digest (1955) 4 (9): Mg-19.
Published: 01 September 1955
... ELEKTRON ZW3 is a high strength wrought magnesium alloy. It shows improved hot formability; it is free from stress-corrosion cracking in service and is readily weldable by the argonarc and heliarc machine processes and by the manual method for simple joints. This datasheet provides information...
Journal Articles
Alloy Digest (1955) 4 (3): Mg-16.
Published: 01 March 1955
... ELEKTRON ZW1 is similar to ELECTRON ZW3 but with reduced zinc content to confer complete freedom from junction cracking in manual argonarc or heriarc welding, with but small sacrifice in strength properties. This datasheet provides information on composition, physical properties, hardness...