Alloy Digest (2009) 58 (3): Mg-76.
Published: 01 March 2009
... Elektron WE43 was developed by Magnesium Elektron for use to 300 deg C and has good mechanical properties at these temperatures. The alloy is used in military and motorsport applications where these properties are at a premium. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2009) 58 (4): Mg-77.
Published: 01 April 2009
... of this alloy (that is, in excess of 1000 h) at temperatures in the range 100 250 °C may result in the loss of ductility. An alternative alloy is Elektron WE43. Applications: The excellent retention of properties at elevated temperatures and improved corrosion resistance will be of interest to designers...