1-1 of 1 Search Results for

Edgar Allen VS4

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1965) 14 (6): TS-166.
Published: 01 June 1965
... Edgar Allen VS4 is a high carbon, water hardening tool steel recommended for cold heading dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat...