Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (6): Ni-372.
Published: 01 June 1989
... EVANOHM alloy R is an electrical resistance alloy with exceptional stability. Its resistivity increases during heat treatment and once obtained does not change significantly even when used at temperatures as high as 392 F (200 C). Resistors made with EVANOHM alloy R show a maximum drift of 5ppm...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1997) 46 (4): Ni-524.
Published: 01 April 1997
... HPM Evanohm R is a nickel-base alloy having low-temperature coefficient of resistance and high electrical resistivity. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: Ni-524. Producer or source: Hamilton Precision Metals Inc. Producer...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (7): Ni-373.
Published: 01 July 1989
... EVANOHM alloy S offers optimum stability and flexibility with regard to both size and required temperature coefficient of resistance. Its extremely low electromotive force vs copper together with its high electrical resistivity are highly desirable properties in a precision resistance wire...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1960) 9 (4): Ni-57.
Published: 01 April 1960
... EVANOHM is a nickel-base alloy having low temperature coefficient of resistance and high electrical resistivity. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on joining. Filing Code: Ni-57. Producer...