1-2 of 2 Search Results for

ESCO no. 56

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1960) 9 (9): Ni-60.
Published: 01 September 1960
... ESCO No. 56 is a nickel-base alloy containing chromium and iron. It is austenitic and has exceptionally high resistance to corrosion, cyclic heating, and oxidation. It is of the 60 Ni-12Cr type alloy. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1966) 15 (5): Co-48.
Published: 01 May 1966
... operations. MACHINING RECOMMENDATIONS Turning Facing - - Back rake, deg. 0 -6 End relief, deg. 6 6 Roughing speed, sfpm 56 49 Finishing speed, sfpm 65 23 Depth of cur 0.08 0.06 Feed, ipr 0.004 ipr 0.012-0.016 in/run Cutting fluid Soluble oil Unlubricated Weldability: ESCO Alloy 72 can be welded to itself or...