Alloy Digest (1962) 11 (3): SA-126.
Published: 01 March 1962
... ESCO Alloy 12M is a low alloy, medium carbon content, hard, shock and impact-resisting steel recommended for heavy duty cast parts. Minor chemical composition variations and heat treatment are employed in order to develop specific properties. This alloy possesses exceptional toughness at low...