1-2 of 2 Search Results for

ENDURO AA

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1953) 2 (6): SS-9.
Published: 01 June 1953
... ENDURO AA is a ductile, non-hardening alloy containing 14 to 18 percent chromium with carbon under 0.12 per cent. It has mechanical properties equal to high grade medium carbon steel, with high resistance to general corrosion and oxidation at high temperatures. This datasheet provides information...
Journal Articles
Alloy Digest (1955) 4 (10): SS-35.
Published: 01 October 1955
... ENDURO AA-FM is a free-machining chromium type stainless steel equivalent to AISI Type 430-F. It is ferritic and non-hardenable. It is corrosion and heat resistant. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...