Alloy Digest (1957) 6 (12): SS-65.
Published: 01 December 1957
... ENDURO 202 is a non-hardenable austenitic chromium-nickel-manganese stainless steel having similar mechanical properties and corrosion resistance to AISI Type 302 stainless steel. It is a general purpose corrosion resisting steel. This datasheet provides information on composition, physical...