Alloy Digest (1960) 9 (8): SS-106.
Published: 01 August 1960
... ENDURO 18-8-SCb is an 18-8 type stainless steel stablized by columbium for increased resistance to intergranular attack. It is recommended for heavy welded equipment and for service within the range of 800-1650 F when corrosive conditions exist. This datasheet provides information on composition...